Sign In | Join Free | My uabig.com |
|
Brand Name : SPEZILLA
Model Number : UNS S32760
Certification : ISO9001;2008
Place of Origin : CHINA
MOQ : Negotiation
Price : Negotiation
Payment Terms : L/C, T/T
Supply Ability : 1000TONS/MONTH
Delivery Time : 15 DAYS
Packaging Details : BUNDLES ,WOODEN BOXES
Product Name : Stainless Steel Duplex Tube
Standard : ASTM A928
Grade : UNS S32760
Produce : WELDED
Welding : EFW
Size : 219.00MM - 2540.00MM
WT : 1.0-5.0mm
Length : 20ft
Test : RT%
Shape : Round
Package : Wooden Case
Application : Heat Exchanger
UNS S32760 Welded duplex stainless steel grade 2205 EFW Gas Stress Corrosion
Super Duplex UNS S32760 has excellent corrosion resistance to a wide variety of media, with outstanding resistance to pitting and crevice corrosion in seawater and other chloride containing environments, with Critical Pitting Temperature exceeding 50°C.
Providing higher strength than both austenitic and 22% Cr Duples Stainless Steels UNS S32760 is suited to a variety of applications in industries such as Chemical Processing, Oil & Gas, and Marine environments.
Applications:
Chemical Process Industry:
Nitric Acid Processes, Polypropylene Production, PVC Production, Dioxide, Caustic Evaporators, Equipment
Handling Organic and Fatty Acids
Marine Industry and Shipbuilding:
Propellers and Shafts, Rudders, Shaft Seals, Pumps, Bolts and Fasteners, Valves, Instrumentation, Oil and Chemical Tankers
Oil and Gas Industry:
Pumps, Valves, Pipe, Vessels, Wellhead Equipment, Subsea Equipment
Pollution Control:
Fans and pumps, Wet Scrubbers, Incinerators
Pulp and Paper Industry:
Black liquor heater tubes, Digester Blow Valves, Rotary Feed Valves, I.D.Fans, Brownstock Washers, Precipitators, Bleaching Components
Food Industry:
Sugar Cane Centrifuges, Corn and Vegetable processing plant
Agrochemicals:
Fertiliser Production (Wet phosphoric acid)
Civil Engineering:
Sewage Treatment
Chemical Composition of UNS S32760 Super Duplex Stanless Steel Pipes and Tubes
Elements | C | Cr | Cu | Fe | Mo | Mn | N | Ni | P | S | Si | W |
Minimum | | 24.0 | 0.5 | REMAINDER | 3.0 | | 0.20 | 6.00 | | | | 0.50 |
Maximum | 0.030 | 26.00 | 1.0 | | 4.0 | 1.0 | 0.30 | 8.00 | 0.030 | 0.010 | 1.00 | 1.00 |
Mechanical Properties of UNS S32760 Super Duplex Stanless Steel Pipes and Tubes
0.2% Proof Stress (N/mm2 ) [ksi] minimum | 550 [79.8] |
Ultimate Tensile Strength (N/mm2) [ksi] minimum | 750 [108.8]] |
Elongation (%) minimum | 25 |
Hardness (HBN) | 270max |
Reduction of Cross Section Area (%) minimum | 45 |
Charpy V-notch Impact at ambient Temp (J) [ft.lb] | 80min [59min] |
Charpy V-notch Impact at -46°C (J) [ft.lb] | 45av, 35min [33av, 25.8min] |
Physical Properties of UNS S32760 Super Duplex Stanless Steel Pipes and Tubes
Density (Kg.m-3) | 7810 |
Magnetic Permeability | 33 |
Young’s Modulus (N/mm2) | 199 x 103 |
Fracture Toughness, KQ (MPa.m½) | 98 |
Specific Heat, 20°C (J.Kg-1.°K-1) | 475 |
Specific Electrical Resistance, 20°C (µO.m) | 0.80 |
Thermal conductivity, 20°C (W.m-1.°K-1) | 14.2 |
Mean coefficient of thermal expansion, 20-100°C (°K-1) | 11.1 x 10-6 |
ASTM A928 UNS S32760 Super Duplex Stainless Steel EFW pipes Specifications
Pipe Range | 6NB to 1200NB - SCH. 5, 10, 20, 30, 40, 60, 80, 100, 120, 140, 160, XXS. |
---|---|
PipeType | Round, Square, Rectangle, Hydraulic, Honed Tubes |
Stainless Steel Pipe | ASTM A312, A358, A269, A270- TP 304, 304L, 304H, 316, 316L, 316H, 316Ti, 309, 310, 317L, 321, 347, 904L. |
TEST CERTIFICATES | MTC, IBR & Third Party Inspection. |
![]() |
UNS S32760 Welded duplex stainless steel grade 2205 EFW Gas Stress Corrosion Images |